Sigh. Cracked one of the clamshell halves. And lo and behold noticed that the whole receiver was crooked AF when looking down the rail.

PAHT-CF. P1S. Dried 85C for 12 hours in AMS-HT, annealed at 90C for 4 hours, sat in plastic bag with wet paper towels to remoisturize for a couple days, then sat idle for another day before working with it.

Dunno whether to try again in PAHT-CF or say fuck it and print in PLA.


Source: https://b.thumbs.redditmedia.com/JTCId1VarL285He--YCOqMJYDVbwVJIsxq4eopGkaAU.jpg